<?xml version='1.0' encoding='UTF-8'?>
<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd">
  <responseDate>2026-05-01T08:29:04Z</responseDate>
  <request metadataPrefix="oai_dc" identifier="oai:meral.edu.mm:recid/906" verb="GetRecord">https://meral.edu.mm/oai</request>
  <GetRecord>
    <record>
      <header>
        <identifier>oai:meral.edu.mm:recid/906</identifier>
        <datestamp>2021-12-13T01:43:09Z</datestamp>
        <setSpec>1582963739756:1582967025340</setSpec>
        <setSpec>user-um</setSpec>
      </header>
      <metadata>
        <oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns="http://www.w3.org/2001/XMLSchema" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
          <dc:title>Fabrication of Titanium Dioxide Nanotubes Array For Photoanode in Mesoscopic Solar Cells</dc:title>
          <dc:creator>Min Min Thein</dc:creator>
          <dc:creator>Min Khant Ko</dc:creator>
          <dc:creator>Hlaing Min</dc:creator>
          <dc:creator>Nyein Wint Lwin</dc:creator>
          <dc:creator>Than Zaw Oo</dc:creator>
          <dc:description>One dimensional (1D) nanostructures have been attracting the research interest and have many&#13; potential applications including mesoscopic solar cells. In this work, 1D titanium dioxide&#13; (TiO2) nanotubes array have been fabricated by the electrochemical anodization of Ti foils in&#13; electrolyte. Focus was placed on the morphology and size control of TiO2 nanotubes by&#13; varying fluoride content in electrolyte (0.3-0.6 Wt%). Fluoride contents of 0.4 and 0.5 Wt%&#13; are optimum for production of well-defined nanotubes array with uniform size distribution&#13; (tube diameter of 100 - 140 nm). It is also observed that higher the fluoride concentration, the&#13; larger is the anodization current across the sample. The tube morphology and size are strongly&#13; sensitive to the fluoride content in electrolyte.</dc:description>
          <dc:date>2016</dc:date>
          <dc:identifier>http://hdl.handle.net/20.500.12678/0000000906</dc:identifier>
          <dc:identifier>https://meral.edu.mm/records/906</dc:identifier>
        </oai_dc:dc>
      </metadata>
    </record>
  </GetRecord>
</OAI-PMH>